Export office · Kunming, China Markets · Southeast Asia / CIS / Middle East / Africa
Home
About
Standards
Applications
Quality
Resources
Contact
Request a quote
Home/Quality

Quality & certification

A pipe either passes the test or it does not — there is no third answer. This page shows where the checks happen, what is recorded, and which documents leave the factory with the container.

SystemISO 9001 · certificate on request
ProductEN · ASTM · DIN · ISO
InspectionIn-house + third party
RecordsPer batch, per shipment
01 / Inspection chain

Five gates before
the container closes

Five gates · photographed at each stage
01
Incoming material

Density, MFI, carbon black, moisture and thermal stability on every compound batch.

02
In-process

Wall thickness, OD and ovality sampled at fixed intervals; parameters logged per run.

03
Finished product

Hydrostatic test, drop impact, Vicat softening and dimensional check against the standard.

04
Pre-shipment

Quantity, marking, packing and loading plan verified before the truck leaves the yard.

Third-party inspection welcome. SGS, BV, Intertek or your own QC team — we schedule the visit, open the batch, and provide the samples. Testing is against the standard written in your purchase order.
02 / Standards & documents

What ships with the pipe

Every consignment leaves with the paperwork a customs broker and a site engineer both ask for. The test report is issued against the standard on your order, not a generic one.

StandardScopeDocument issued per order
ISO 9001Quality management system of the producing plantMill certificate
EN 1452 / ISO 1452PVC-U pressure systems for waterDimensional + hydrostatic test report
ASTM D1785 / F441PVC-U Sch 40 / 80 · CPVC Sch 80Dimensional + test report
ISO 15874 / DIN 8077PP-R hot & cold water systemsTest report
ISO 4427 / EN 12201PE 100 water supplyTest report
CJ/T 445PVC-O 500 grade, DN 90–630Test report
Export setEvery shipmentPacking list · invoice · CO / Form E
03 / Laboratory

What sits in the lab

The equipment list is short and specific. If a test cannot be run in house, it goes to a third-party lab and the report is quoted in the offer.

  • HydrostaticLong-term pressure test rig, 20 – 95 °C
  • ImpactDrop weight tester, 0 °C and 23 °C conditioning
  • ThermalVicat softening point, dimensional stability at 150 °C
  • MaterialDensity, MFI, carbon black content, moisture analyser
Lab Laboratory and inspection
04 / Packing & loading

How it arrives
matters as much

Pipe is cheap to make and expensive to replace. Packing is specified per diameter, per container and per destination climate.

01

Bundles

Strapping at fixed spacing for small and medium diameters; load plan issued per container size.

02

Neutral or branded

Plain packing for traders, buyer-branded printing for distributors. Marking agreed on the PI.

03

UV protection

Wrapping for above-ground storage in high-insolation destinations.

04

Loading photos

Container interior photographed before closing, sent with the shipping documents.

Need a test report
before you order?

Tell us the standard and the diameter — we send the current batch report, not a marketing brochure.